Abstract

A co-doped silicate optical waveguide having a core including silica, and oxides of aluminum, germanium, erbium and thulium. The composition concentrations are: Er from 15 ppm to 3000 ppm; Al from 0.5 mol % to 12 mol %; Tm from 15 ppm to 10000 ppm; and Ge from 1 mol % to 20 mol %. In a specific embodiment, the concentration of Er is from 150 ppm to 1500 ppm; Al is from 2 mol % to 8 mol %; and Tm is from 15 ppm to 3000 ppm. A boron-less cladding surrounds the core.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 17.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A silicate optical waveguide comprising: a) a core comprising silica, and oxides of Al, Ge, Er, and Tm; i) wherein the concentration of Er is from 15 ppm to 3000 ppm, ii) the concentration of Al is from 0.5 mol % to 12 mol %, iii) the concentration of Tm is from 15 ppm to 10000 ppm, and iv) the concentration of Ge is from 1 mol % to 20 mol %; and b) a boron-free cladding immediately surrounding the core.

  2. Claim 2Depends on #1

    The waveguide of claim 1 , wherein a) the concentration of Er is from 150 ppm to 1500 ppm; b) the concentration of Al is from 2 mol % to 8 mol %; and c) the concentration of Tm is from 15 ppm to 3000 ppm.

  3. Claim 3Depends on #1

    The waveguide of claim 1 , wherein the concentration of Er is from 150 ppm to 1500 ppm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Lucent Technologies announces two new erbium-doped fibers for the extended L-band the C-band"; Lucent Technologies [online]; [available on the internet Oct. 1, 2001]; [retrieved from the internet Jan. 23, 2003].
  • A. Mori, et al; "1.5 mum Broadband Amplification by Tellurite-Based EDFAs"; Conference on Optical Fiber Communications, Technical Digest, Postconference Ed. OSA Technical Digest Series vol. 6; 1997; pp. 371-374; Optical Society of America.
  • A. Mori, et al; "1.5 μm Broadband Amplification by Tellurite-Based EDFAs"; Conference on Optical Fiber Communications, Technical Digest, Postconference Ed. OSA Technical Digest Series vol. 6; 1997; pp. 371-374; Optical Society of America.
  • Dianov, E.M., et al; "Application of Reduced-Pressure Plasma CVD Technology to the Fabrication of Er-doped Optical Fiber", Optical Materials (Aug. 1994); vol. 3, No. 3, Amsterdam; pp. 181-185, no date.
  • H. Jeong & K. Oh; "Characterization of Amplified Spontaneous Emission Light Source from an Er<3+>/Tm<3+> Co-doped Silica Fiber"; Conference on Lasers and Electro-Optics, Technical Digest, Postconference Ed. TOPS vol. 39; 2000; pp. 544-545; Optical Society of America.