Patents
US 6,753,133 B2#25336930 Most CitedExpiredUnited States (USPTO)Utility

Method and manufacturing a semiconductor device having a ruthenium or a ruthenium oxide

4Forward Citations (#25336930 Global)
0.2/yrCitation Velocity (#35292988 Global)
1.31Citation PageRank (#28061453 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for fabricating a semiconductor device includes the following steps. At first, a Ru or RuO 2 film and a SiO 2 layer are formed over a Si substrate in that order. Then, a resist pattern is formed on the SiO 2 layer and is then provided as a mask to etch the SiO 2 layer to form a contact hole. The Ru or RuO 2 film is exposed at the bottom of the contact hole. Subsequently, a plasma ashing is performed using an ashing gas prepared by mixing O 2 with N 2 where the composition ratio of N 2 is 50% or more at a substrate temperature of 200° C. or more for ashing the resist pattern. Consequently, the present invention allows the ashing of the resist pattern over the Ru or RuO 2 film at a high selectivity to prevent the Ru or RuO 2 film from becoming disappeared.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a semiconductor device including at least one of a ruthenium and a ruthenium oxide, comprising: ashing a photo-sensitive material over the ruthenium or the ruthenium oxide using a gas mixture containing oxygen gas or ozone gas and nitrogen gas, wherein the percentage composition of nitrogen gas is 50% or more.

  2. Claim 2Depends on #1

    The method as claimed in claim 1 , wherein the ashing is performed by heating a substrate over which the ruthenium or the ruthenium oxide is formed at a temperature of 200° C. or more.

  3. Claim 3Depends on #1

    The method as claimed in claim 1 , wherein the ashing is performed after etching an interlayer insulation film on the ruthenium or the ruthenium oxide using the photo-sensitive material as a mask.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗