Patents
US 6,749,693 B2#33549501 Most CitedExpiredUnited States (USPTO)Utility

Method of producing (110)[001] grain oriented electrical steel using strip casting

3Forward Citations (#33549501 Global)
0.1/yrCitation Velocity (#39753930 Global)
1.03Citation PageRank (#40174745 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In a method of producing a strip suitable for further processing to yield a (110)[001] grain oriented electrical steel from a thin strip such as a continuously cast thin strip the thin cast strip is processed to promote recrystallization from the surface layer of the strip (S=0) into the quarter thickness of the strip (S=0.2 to 0.3). The process parameters are selected so that the strain/recrystallization parameter (K*)<-1>, >=about 6500 andwherein,THBA is the annealing temperature of the strip (in °Kelvin),THR is the hot rolling temperature of the strip (in °Kelvin),{dot over (epsilon is the strain rate of hot rolling,ti is the initial thickness of the strip before hot rolling, andtf is the final thickness of the strip after hot rolling.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a strip suitable for further processing to yield a (110)[001] grain oriented electrical steel comprising the steps of: a. obtaining a strip having an initial thickness of ≦0.39 in (10 mm); b. hot rolling the strip of step a; c. annealing the strip of step b; and d. having a strain/recrystallization parameter, (K*) −1 , ≧about 6500; wherein, ( K * ) - 1 = ( T HBA )  ln  [ e . 0.15  exp  ( 7616 T HR )  ln  ( t c t f )

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗