US 6,747,445 B2#898571 Most CitedExpiredUnited States (USPTO)Utility

Stress migration test structure and method therefor

51Forward Citations (#898571 Global)
2.3/yrCitation Velocity (#1541819 Global)
8.11Citation PageRank (#1501932 Global)
19Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A stress migration test structure is provided that can be used to detect stress migration defects in traces or conductors of integrated circuits. The stress migration test structure can be placed between die areas on a wafer, or on a die. On the die, a stress migration test structure can be placed in otherwise unused areas of a die such as between bond pads and the periphery of a die, in a layer beneath bond pads, in a region between the bond pads and the perimeter of standard area for circuit layout, or in regions in more than one level of the integrated circuit. The stress migration test structure may also be placed within the standard area for circuit layout and used, with some additional circuitry, as a stress migration test structure on an integrated circuit once the die is packaged. Obtaining information from the impedance segments of a stress migration test structure can be accomplished employing either a mechanical stepping or an electrical stepping technique.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 51.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A wafer, comprising: at least two die areas formed on the wafer, the at least two die areas defining a street therebetween; and a stress migration test structure in the street, the stress migration test structure comprising a conductive runner having a length sufficient to develop axial stress above the threshold for nucleating voids for the technology in which the runner is fabricated, the conductive runner having a plurality of taps at uniform impedance intervals along the runner, the taps spaced along the runner such that the variation of the impedance of the runner between adjacent taps, d

  2. Claim 2Independent Claim

    A wafer, comprising: at least four die areas formed on

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 51 total)

Non-Patent Literature (5)

  • Circuits and Devices, "Stress-Voiding of Narrow Conductor Lines," F. G. Yost and F. E. Campbell, 1990 IEEE, pp. 40-44.
  • Hinode et al., "Mechanism of Stress-Induced Migration", Jun. 1988, VLSI Multilevel Interconnection Conference, 1988. Proceedings., Fifth International IEEE, pp. 429-435.*
  • Hoang et al., "Wafer Level Reliability Assessment of Stress-Induced Voiding", Jun. 1991, VLSI Multilevel Interconnection Conference, 1991, Proceedings. Eighth International IEEE, pp. 387-389.*
  • Journal of Electronic Materials, vol. 24, No. 6, 1995, "Enhanced Stress-Migration Reliability for ULSI Interconnect: An Insight into the Perils of Screening Al Depositions Based on Grain Size," V. Ryan et al., pp. 969-974.
  • Matsunaga et al., "Accurate, Non-Time-Intensive Evaluation of the Stress-Migration Endurance for Layered Al Interconnects", Apr. 1994, Reliability Physics Symposium, 1994. 32<nd >Annual Proceedings., IEEE International, pp. 256-260.*