Polypropylene molding composition for the production of moldings having a decorative surface
Abstract
Polypropylene molding composition for the production of moldings having a decorative surface A polypropylene molding composition containing from 0.3 to 3% by weight of carbon fibers having a fiber length of from 0.5 to 18 mm can be converted into moldings having a decorative surface. These moldings are used, in particular, in the interior of motor vehicles, but are also suitable for other applications.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A polypropylene molding composition for the production of moldings having a decorative surface appearance, containing a polymer of propylene, from 0.3 to 3% by weight, based on the molding composition, of carbon fibers having a fiber length of from 0.5 to 18 mm, and from 10 to 50% by weight, based on the molding composition, of talc.
- Claim 2Depends on #1
The molding composition as claimed in claim 1 , wherein said polymer of propylene comprises: a) from 50 to 95% by weight of isotactic polypropylene or a copolymer of propylene with up to 10% by weight of ethylene; and b) from 5 to 50% by weight of an ethylene/propylene rubber which is compatible with polypropylene.
- Claim 3Depends on #2
The molding composition as claimed in claim 2 , wherein said polymer of propylene comprises: a) from 70 to 90% by weight of isotactic p
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (2)
- JP-A 58 155 925 (Idemitsu Petrochem) Sep. 16, 1983.
- Polypropylene (properties and applications), D. B. Iwanukow and M. L. Friedman, p. 154, 1974. (Abstract).