Thermoelectric material improved in figure of merit, process for producing thereof and peltier module using the same
Abstract
Thermoelectric material of (Bi, Sb)(Te, Se) system is produced through a liquid quenching method and an extrusion from a die unit having an inlet portion and an outlet portion crossing each other at 30-150 degrees so that the crystal grains have an average grain size equal to or less than 30 microns and (001) planes mostly oriented in parallel to a direction in which electric current to flow, thereby achieving the figure of merit equal to or greater than 3.0×10 −3 /K.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 25.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A thermoelectric material composed of at least one element selected from the group consisting of Bi and Sb and at least one element selected from the group consisting of Te and Se, and comprising crystal grains having respective [001] directions and an average grain size equal to or less than 30 microns, certain crystal grains having the [001] directions crossing a direction in which an electric current flows at 45 degrees or less, said certain crystal grains occupying an area equal to or less than 10% on a section perpendicular to said direction, said thermoelectric material having a density
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 25 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (2)
- Proceeding of 200 Spring conference of Japan Society of Powder and Powder Metallurgy, p. 197, no month provided.
- S. Miura, et al., "Texture and Thermoelectric Properties of Hot-Extruded Bi2Te3 Compound", Materials Science and Engineering A277 (2000), pp. 244-249, no moth provided.