Process for forming a metal oxy-nitride dielectric layer by varying the flow rate of nitrogen into the chamber
Abstract
The invention relates to a semiconductor device and the process of forming a metal oxy-nitride gate dielectric layer or a metal-silicon oxy-nitride gate dielectric layer. The metal oxy-nitride or metal-silicon oxy-nitride dielectric layer comprises at least one of a metal, silicon, oxygen, and nitrogen atoms where the nitrogen to oxygen atomic ratio is at least 1:2. The metal oxy-nitride or metal-silicon oxy-nitride material has a higher dielectric constant in comparison with a silicon dioxide, providing similar or improved electrical characteristics with a thicker thickness. Other benefits include reduced leakage properties, improved thermal stability, and reduced capacitance versus voltage (CV) hysteresis offset.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 2.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for forming a semiconductor structure comprising: placing a substrate into a chamber, wherein the substrate includes a semiconductor region; and physically vapor depositing a dielectric layer that contacts the semiconductor region, wherein: depositing includes: flowing nitrogen atoms into the chamber at a first nitrogen atomic flow rate at a first time period; and flowing nitrogen atoms into the chamber at a second nitrogen atomic flow rate at a second time period after the first time period, wherein the second nitrogen atomic flow rate is substantially different from the first nitro
- Claim 2Depends on #1
The process of claim 1 , wherein the first nitrogen atomic flow rate is higher than the
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 6,933,189 B2 | Integration system via metal oxide conversion | 2005 | 1 |
| US 2004224471 A1 | Integration system via metal oxide conversion | — | 4 |
References Cited — Backward Prior Art (15)
Non-Patent Literature (5)
- Collard, "Growth of nitrogen stabilised cubic ZrO2 phase by reactive magnetron sputtering using two reactive gases," Elsevier Science Ltd., pp. 153-157 (1999).
- Jung et al., "Electrical and Reliabilty Characteristics of an Ultrathin TaOxNy Gate Dielectric Prepared by ND3 Annealing of Ta2O5<1>" IEEE Electron Device Letters, vol. 21, No. 12, Dec. 2000.
- Jung et al., "Electrical and Reliabilty Characteristics of an Ultrathin TaOxNy Gate Dielectric Prepared by ND3 Annealing of Ta2O51" IEEE Electron Device Letters, vol. 21, No. 12, Dec. 2000.
- Lee et al., "Ultrathin Hafnium Oxide with Low Leakage and Excellent Reliability for Alternative Gate Dielectric Application," Microelectronics Research Center, University of Texas, Austin (4 pgs.).
- Nieh et al., "MOSCAP and MOSFET characteristics using ZrO2 gate dielectric deposited directly on Si," Microelectronics Research Center, University of Texas, Austin (4 pgs.).