Self-constrained low temperature glass-ceramic unfired tape for microelectronics and methods for making and using the same
Abstract
A monolithic self-constrained green body tape for use in low temperature ceramic co-firing is provided. The tape contains at least two layers: one low temperature ceramic layer containing particles of a glass, a ceramic, and an organic binder, and a self-constraining layer containing a refractory ceramic and a wetting agent for the glass in the first layer. When the tape is fired at a sintering temperature of the low temperature ceramic layer, densification occurs in the z (thickness) direction, but essentially no shrinkage (less than about 1%) occurs in the x-y planes. A method for forming a multilayer green body tape using simultaneous wet on wet ceramic slurry deposition is also provided. A dense, monolithic, low temperature, co-fired, self-constrained, multicomponent structure is also provided. The structure contains at least two multilayer ceramic substrates having electronic circuit components mounted thereon or therein. Each multilayer ceramic substrate contains at least two layers with one being a self-constraining layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 43 · Forward citations: 23.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A monolithic green body tape having an x-y plane and a thickness in a z-direction for use in low temperature ceramic co-firing, comprising: at least one low temperature ceramic layer containing particles of a first ceramic, a first glass, and a first organic binder; and at least one self-constraining layer containing particles of a refractory ceramic, a wetting agent for the first glass, and a second organic binder; wherein the refractory ceramic will not sinter at a sintering temperature of the low temperature ceramic layer, such that upon firing of the green body tape at the sintering temper
- Claim 2Depends on #1
The tape according to claim 1 , wherein the g
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 23 total)
References Cited — Backward Prior Art (43)
Non-Patent Literature (3)
- Excerpt from Ragan Technologies, Inc., "ZST(TM)-LTCC In-House/Green Tape Production", web site http://www.ragantech.com/CIA.html, Jan. 22, 2002.
- Excerpt from Ragan Technologies, Inc., "ZST™—LTCC In-House/Green Tape Production", web site http://www.ragantech.com/CIA.html, Jan. 22, 2002.
- Excerpt from SMI-ED Ogaki Ceramics, Inc., "Low Temperature Fireable Ceramics", web site http://www.smiedoc.co.jp/elfc01.html, Jan. 22, 2002.