Patents
US 6,743,396 B2#6926813 Most CitedExpiredUnited States (USPTO)Utility

Method for producing AlMn strips or sheets

14Forward Citations (#6926813 Global)
0.6/yrCitation Velocity (#12303889 Global)
2.53Citation PageRank (#9950999 Global)
14Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a method for producing AlMn strips or sheets for producing components by soldering, wherein a precursor material is produced from a melt which contains (in weight-percent) Si: 0.3-1.2%, Fe: ≦0.5%, Cu: ≦0.1%, Mn: 1.0-1.8%, Mg: ≦0.3%, Cr+Zr: 0.05-0.4%, Zn: ≦0.1% , Ti: ≦0.1% , Sn: ≦0.15%, and unavoidable companion elements, whose individual amounts are at most 0.05% and whose sum is at most 0.15%, as well as aluminum as the remainder, wherein the precursor material is preheated at a preheating temperature of less than 520° C. over a dwell time of at most 12 hours, wherein the preheated precursor material is hot rolled into a hot strip using a final hot rolling temperature of at least 250° C., wherein the hot strip is cold rolled into a cold strip without intermediate annealing.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 14.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    0 to 1.8% Mn; not more than 0.3% Mg; a sum of Cr and Zr in the range 0.05 to 0.4%; not more than 0.1% Zn; not more than 0.1% Ti; not more than 0.15% Sn; unavoidable companion elements; and aluminum as the remainder; wherein any one of said unavoidable companion elements individually amounts to at most 0.05%; and all of said unavoidable companion elements collectively amount to at most 0.15%; and wherein the ratio of weight percent Sn to weight percent Si is not less than 0.03; preheating s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗