Polyester having improved crystallization behavior and extrusion blow molded articles made therefrom
Abstract
A PCT copolyester composition having at least about 70 mole % terephthalic acid and at least about 70 mole % 1,4-cyclohexanedimethanol and an inherent viscosity of greater than about 0.9 dL/g is prepared by solid state polymerizing a copolyester composition having a starting inherent viscosity of from about 0.4 to about 0.8 dL/g for a period of from about 1 minute to 100 hours and at a temperature of from about 140° C. to about 2° C. below the melting point of the copolyester to produce a copolyester having an inherent viscosity of greater than about 0.9 dL/g. Another aspect of the present invention is an extrusion blow molded article made from the copolyester prepared by the solid state polymerization process.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 19.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A copolyester comprising at least about 70 mole % terephthalic acid and at least about 70 mole % 1,4-cyclohexanedimethanol wherein the mole percentages of the acid component total 100 mole % and the mole percentages of the glycol component total 100 mole %; wherein said copolyester has a inherent viscosity greater than about 0.9 dL/g and is prepared by a process comprising solid-state polymerizing a copolyester having a starting inherent viscosity of from about 0.4 to about 0.8 dL/g for a period of from about 1 minute to 100 hours and at a temperature of from about 140° C. to about 2° C. below
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗