Patents
US 6,740,291 B2#16101332 Most CitedExpiredUnited States (USPTO)Utility

Ni-Cr-Mo alloys resistant to wet process phosphoric acid and chloride-induced localized attack

7Forward Citations (#16101332 Global)
0.3/yrCitation Velocity (#24966562 Global)
1.33Citation PageRank (#27627136 Global)
13Prior Art Cited
3Claims (3 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A nickel-chromium-molybdenum alloy that is thermally stable and resistant to wet process phosphoric acid and chloride induced localized attack contains in weight percent 31.0 to 34.5% chromium, 7.0 to 10.0% molybdenum, up to 0.2% nitrogen, up to 3.0% iron, up to 1.0% manganese, up to 0.4% aluminum, up to 0.75% silicon, up to 0.1% carbon with the balance nickel plus impurities.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 7.

Claims (3 — 3 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A nickel-chromium-molybdenum alloy resistant to wet process phosphoric acid and chloride-induced localized attack, consisting essentially of:

  2. Claim 7Independent Claim

    0 to 9.0 wt. % Molybdenum Up to 0.2 wt. % Nitrogen Up to 3.0 wt. % Iron Up to 1.0 wt. % Manganese

  3. Claim 31Independent Claim

    7 to 34.5 wt. % Chromium

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗