The present invention provides a system for preventing excess silicon consumption in a semiconductor wafer by depositing a metal layer ( 114 ) on top of a native oxide layer above a silicide layer ( 110 ) of the semiconductor wafer and then reducing the native oxide layer to form low resistance contacts. The native oxide layer is reduced using a rapid thermal annealing process within a temperature range to preserve the integrity of the silicide layer ( 110 ) and reduce excess silicon consumption. The temperature range can be greater than 350° C. and less than 615° C., but is optimal between 485° C. to 550° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for preventing excess silicon consumption in a semiconductor wafer, comprising the steps of: depositing a metal layer on top of a native oxide layer that resides upon a silicide layer; and reducing the native oxide layer to form low resistance contacts, using a rapid thermal annealing process within a temperature range greater than 350° C. and less than 615° C.

  2. Claim 2Depends on #1

    The method as recited in claim 1 , wherein the temperature range is about 485° C. to 550° C.

  3. Claim 3Depends on #1

    The method as recited in claim 1 , wherein the temperature range is approximately 485° C.