Abstract
The present invention relates to a polycarbonate which can be obtained by a melting method and has a viscosity-average molecular weight of 16000 to 27000, and whose loss angle delta and complex viscosity eta* (Pa.s) measured under the conditions of 250° C. and an angular velocity of 10 rad/s satisfy the following relation (1):
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 5.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A polycarbonate which can be obtained by a melting method using an aromatic dihydroxyl compound and a carbonic acid diester as starting materials and has a viscosity-average molecular weight of 16000 to 27000, and whose loss angle δ and complex viscosity η* (Pa·s) measured under the conditions of 250° C. and an angular velocity of 10 rad/s satisfy the following relation (1): 4,700≦Tan δ/(η*) −0.87 (1).
- Claim 2Depends on #1
A polycarbonate according to claim 1 having a terminal OH group content in the range of 50 to 1,000 ppm.
- Claim 3Independent Claim
A polycarbonate resin composition comprising a polycarbonate which can be obtained by a melting method using an aromatic dihydroxyl compound and a carbonic acid diester as starting material and has a viscosity-average molecular weight of 16000 to 27000