Patents
US 6,730,160 B2#16123579 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacture of structural insulating building materials

7Forward Citations (#16123579 Global)
0.3/yrCitation Velocity (#24968699 Global)
1.30Citation PageRank (#28402181 Global)
20Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A fire retardant building material composed of a mixture of water and cellulose fibers, both of which can be comprised of readily available materials at the job site, such as the available water supply or natural water and scrap shredded paper, including newspaper or other discarded paper or cardboard materials. The water and cellulose fiber is mixed to form a slurry and calcium hydroxide, alumina, salt and ammonia are added. Pigments and aggregates may be added for appearance.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of making a construction material comprising: a. Mixing water and cellulose fibers to form a slurry; b. Mixing salt into the slurry; c. Mixing ammonia into the slurry; d. Mixing calcium hydroxide into the slurry; and e. Mixing alumina into the slurry, wherein the ratio of calcium hydroxide to salt is approximately 25 to 1, by weight, and the ratio of calcium hydroxide to ammonia is approximately 25 to 1, by weight.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein steps b, c, d and e may be performed in any order.

  3. Claim 3Depends on #1

    The method of claim 1 , including the step of pouring the combination created by steps a, b, c, d and e into a form and drying at ambient temperature.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)