High dielectric constant very low fired X7R ceramic capacitor, and powder for making
Abstract
The invention includes a dielectric ceramic powder mixture comprising at least ninety weight percent essentially pure barium titanate powder having an average particle size of from 0.2 to 1.2 microns; from 0.2 to 2.5 weight percent of barium lithium borosilicate flux; from 0.1 to 0.3 weight percent of MnCO 3 ; a grain growth inhibitor such as niobium oxide or other niobate compound; and, 0.4 to 1.2 weight percent of an additive selected from the group consisting of a rare earth oxide, yttrium oxide, a combination of rare earth oxides, and a combination of yttrium oxide and rare earth oxides, such that ions of the additive(s) have an average ionic radius of about 0.97 angstroms. The dielectric ceramic powder provides a start powder for making very low firing multilayer ceramic capacitors satisfying X7R performance requirements.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A dielectric ceramic start powder comprising: a. at least ninety weight percent essentially pure barium titanate powder having an average particle size of from 0.2 to 1.2 microns; b. from 0.2 to 2.5 weight percent of a flux selected from the group consisting of barium lithium borosilicate flux, zinc lithium borosilicate flux, and mixtures thereof; c. from 0.05 to 0.3 weight percent of MnCO 3 ; d. a grain growth inhibitor selected from the group consisting of niobium compounds Nb 2 O 5 , BaNb 2 O 6 , CaNb 2 O 6 , MgNb 2 O 6 , LiNbO 3 , and mixtures thereof such that a weight percent of Nb 2 O 5
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗