Silicide pattern structures and methods of fabricating the same
Abstract
Silicide interfaces for integrated circuits, thin film devices, and backend integrated circuit testing devices are formed using a barrier layer, such as titanium nitride, disposed over a porous, thin dielectric layer which is disposed between a silicon-containing substrate and a silicidable material which is deposited to form the silicide interfaces for such devices. The barrier layer prevents the formation of a silicide material within imperfections or voids which form passages through the thin dielectric layer when the device is subjected to a high temperature anneal to form the silicide contact from the reaction of the silicidable material and the silicon-containing substrate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 0.
Claims (18)
- Claim 1Independent Claim
A method for forming a contact interface, comprising: providing a substrate comprising semiconductor material and including at least one active-device region formed therein; forming a first layer comprising dielectric material over the substrate; forming a second layer comprising barrier material comprising at least one of titanium nitride, tungsten nitride, tungsten silicon nitride, and titanium silicon nitride over the first layer; exposing at least a portion of the at least one active-device region through the first and second layers; introducing an electrically conductive silicidable material onto at least an exposed region of the at least one active-device region; forming a silicide contact at an interface between the electrically conductive silicidable material and the at least the exposed portion of the at least one active-device region; and removing the second layer after forming the silicide contact.
- Claim 2Depends on #1
The method of claim 1 , wherein forming the first layer comprises depositing TEOS.
- Claim 3Depends on #1
The method of claim 1 , wherein forming the second layer comprises depositing titanium nitride.
- Claim 4Depends on #1
The method of claim 1 , wherein introducing the electrically conductive silicidable material comprises disposing cobalt.
- Claim 5Depends on #1
The method of claim 1 , wherein forming the silicide contact comprises annealing the electrically conductive silicidable material and semiconductor material of the exposed region of the at least one active-device region to one another.
- Claim 6Depends on #5
The method of claim 5 , wherein annealing is effected by heating at least the semiconductor material to a temperature of about 400° C. to about 800° C.
- Claim 7Depends on #5
The method of claim 5 , wherein annealing is effected by heating at least the semiconductor material to a temperature of about 450° C. to about 600° C.
- Claim 8Depends on #1
The method of claim 1 , further including removing an unreacted portion of the electrically conductive silicidable material.
- Claim 9Depends on #8
The method of claim 8 , wherein removing the unreacted portion is effected without substantially removing the silicide contact.
- Claim 10Depends on #9
The method of claim 9 , wherein removing said the unreacted portion is effected without substantially removing the barrier material.
- Claim 11Depends on #8
The method of claim 8 , wherein removing the unreacted portion is effected with an HPM solution.
- Claim 12Depends on #1
The method of claim 1 , wherein removing the second layer is effected without substantially removing the silicide contact.
- Claim 13Depends on #12
The method of claim 12 , wherein removing the second layer is effected without substantially removing the first layer.
- Claim 14Depends on #1
The method of claim 1 , wherein removing the second layer comprises substantially completely removing the second layer.
- Claim 15Depends on #1
The method of claim 1 , wherein removing the second layer is effected with an APM solution.
- Claim 16Depends on #1
The method of claim 1 , wherein forming the second layer comprises preventing the electrically conductive silicidable material from reacting with the semiconductor material through at least one of a void and an imperfection in the first layer.
- Claim 17Depends on #1
The method of claim 1 , wherein introducing the electrically conductive silicidable material comprises introducing a material which is different from the barrier material.
- Claim 18Independent Claim
A method for forming a contact interface, comprising: providing a substrate including at least one active-device region formed therein; forming a layer comprising dielectric material over an active surface of the substrate; forming another layer comprising a barrier material comprising at least one of titanium nitride, tungsten nitride, tu
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application is a continuation of application Ser. No. 09/795,882, filed Feb. 28, 2001, now U.S. Pat. No. 6,410,420, issued Jun. 25, 2002, which is a continuation of application Ser. No. 09/136,384, filed Aug. 19, 1998, now U.S. Pat. No. 6,235,630, issued May 22, 2001. BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to contact interfaces on the surface of semiconductor substrates and methods of forming the same. More particularly, the present invention relates to forming silicide interfaces for use with thin film devices and backend integrated circuit (“IC”) testing devices. 2. State of the Art In the processing of integrated circuits, electrical contact must be made to isolated active-device regions formed within a semiconductor substrate, such as a silicon wafer. Such active-device regions may include p-type and n-type source and drain regions used in the production of NMOS, PMOS, and CMOS structures for production of DRAM chips and the like. The active-device regions are connected by conductive paths or lines which are fabricated above an insulative or dielectric material covering a surface of the semiconductor substrate. To provide electrical connection between the conductive path and the active-device regions, openings in the insulative material are generally provided to enable a conductive material to contact the desired regions, thereby forming a “contact.” The openings in the insulative material are typically referred to as “contact openings.” Higher performance, lower cost, increased miniaturization of components, and greater packaging density of integrated circuits are goals of the computer industry. However, as components become smaller and smaller, tolerances for all semiconductor structures (such as circuitry traces, contacts, dielectric thickness, and the like) become more and more stringent. In fact, each new generation o
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (47)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 6,197,646 B1 | Manufacture of semiconductor device with salicide electrode | 2001 | 1 |
Non-Patent Literature (2)
- Badih El-Kareh, "Fundamentals of semiconductor processing technoloies", Klumer Academic Publishers 1995., pp117-118.*
- Harper, Charles A., "Electronic Packaging and Interconnection Handbook," Third Edition (date unknown), p. 1.9, McGraw-Hill.