Abstract

A low-k dielectric metal conductor interconnect structure having no micro-trenches present therein and a method of forming such a structure are provided. Specifically, the above structure is achieved by providing an interconnect structure which includes at least a multilayer of dielectric materials which are applied sequentially in a single spin apply tool and then cured in a single step and a plurality of patterned metal conductors within the multilayer of spun-on dielectrics. The control over the conductor resistance is obtained using a buried etch stop layer having a second atomic composition located between the line and via dielectric layers of porous low-k dielectrics having a first atomic composition. The inventive interconnect structure also includes a hard mask which assists in forming the interconnect structure of the dual damascene-type. The first and second composition are selected to obtain etch selectivity of at least 10 to 1 or higher, and are selected from specific groups of porous low-k organic or inorganic materials with specific atomic compositions and other discoverable quantities.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 24.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a low-k dielectric plus metal conductor interconnect structure which comprises the steps of: (a) forming a multilayer of spun-on dielectrics on a surface of a substrate, said multilayer of spun-on dielectrics including first and second porous low-k dielectrics which are separated from each other by a buried etch stop layer, said first and second porous low-k dielectrics having a first composition, and said buried etch layer is selected from the group consisting of an inorganic dielectric, an inorganic/organic hybrid dielectric, and an organic dielectric with the proviso

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 24 total)

Non-Patent Literature (5)

  • Goldblatt, R.D., et al., "A High Perfomance 0.13 mum Copper BEOL Technology with Low-k Dielectric", Proceedings of 2000 HTC, IEEE, (2000).
  • Goldblatt, R.D., et al., “A High Perfomance 0.13 μm Copper BEOL Technology with Low-k Dielectric”, Proceedings of 2000 HTC, IEEE, (2000).
  • Hasegawa, T., et al., "Copper Dual Damascene Interconnects with Low-K (Keff < 3.0) Dielectrics Using FLARETM and an Organo-Silicate Hard Mask", IEEE. (1999) pp. 26.4.1-26.4.4.
  • Takao, Y., et al., "A 0.11 mum CMOS Technology with Copper and Very-low-k Interconnects for High-Performance System-On-a Chip Cores", IEEE, (2000) pp. 23.1.1-23.1.4.
  • Takao, Y., et al., “A 0.11 μm CMOS Technology with Copper and Very-low-k Interconnects for High-Performance System-On-a Chip Cores”, IEEE, (2000) pp. 23.1.1-23.1.4.