Patents
US 6,716,740 B2#19359925 Most CitedExpiredUnited States (USPTO)Utility

Method for depositing silicon oxide incorporating an outgassing step

5Forward Citations (#19359925 Global)
0.2/yrCitation Velocity (#30679997 Global)
2.20Citation PageRank (#12520282 Global)
16Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for depositing an inter-metal-dielectric layer on a semiconductor substrate by plasma chemical vapor deposition without the layer cracking defect is disclosed. The semiconductor substrate is first heat-treated in the same plasma process chamber to a temperature of at least 300° C. for a length of time sufficient to outgas a surface of the semiconductor substrate. The impurity gases absorbed on the surface of the semiconductor substrate can be effectively outgassed during the heat treatment process such that they are not trapped under an IMD layer deposited in a subsequent plasma deposition process. The method effectively minimizes or eliminates completely the IMD layer cracking defect of the dielectric layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for depositing an inter-metal-dielectric (IMD) layer on a semiconductor substrate by plasma chemical vapor deposition (CVD) comprising the steps of: providing a pre-processed semiconductor substrate; positioning said semiconductor substrate in a plasma CVD chamber; heating said semiconductor substrate in said chamber to a temperature between 300° C. and 400° C. for a length of time sufficient to outgas a surface of said semiconductor substrate; and conducting a plasma CVD process on said semiconductor substrate and depositing said inter-metal-dielectric layer.

  2. Claim 2Depends on #1

    A method for depositing an inter-metal-dielectric layer according to claim 1 , wherein said semiconductor substrate is preferably heated to a temperature between 350° C. and 400° C. during said heating step.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗