Method for preparation of slenderized animal fiber
Abstract
A slenderized crimped animal fiber with a fixed slenderized form having a lowering rate of tensile strength for undyed spun yarn of no less than 10%, fiber contraction in boiling water of no more than 1%, an alkali solubility of no more than 22% by weight and a UB solubility of no more than 35% by weight, wherein the slenderized crimped animal fiber is prepared by being drawn by practically 1.20 to 1.60 times after an anisotropic swelling is given to the animal fiber consisting of bilateral structure using swelling plasticization with base.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for preparation of a slenderized crimped animal fiber with a fixed slenderized form having a lowering rate of tensile strength for undyed spun yarn of no less than 10%, fiber contraction in boiling water of no more than 1%, an alkali solubility of no more than 22% by weight and a UB solubility of no more than 35% by weight, comprising: a) a process wherein an actual twist is applied to an animal fiber sliver; b) a process wherein a twisted animal fiber sliver is swelled and plasticized by a basic aqueous solution and subsequently an anisotropic swelling is given to the animal fiber co
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (2)
- Patent Abstracts of Japan, vol. 2000, No. 16, May 8, 2001 & JP 2001 003238 A (Kurabo Ind. Ltd.), Jan. 9, 2001.
- U.S. patent application Ser. No. 09/902,256 (Hisashi et al.).