Method of producing epitaxial wafers
Abstract
The invention relates to a method of producing epitaxial wafers for the manufacture of high integration density devices capable of showing stable gettering effect. Specifically, it provides (1) a method of producing epitaxial wafers which comprises subjecting a silicon wafer sliced from a single crystal ingot grown by doping with not less than 1×10 13 atoms/cm 3 of nitrogen to 15 minutes to 4 hours of heat treatment at a temperature not lower than 700° C. but lower than 900° C. and then to epitaxial growth treatment. It is desirable that the above single crystal ingot have an oxygen concentration of not less than 11×10 17 atoms/cm 3 . Further, (2) the above heat treatment is desirably carried out prior to the step of mirror polishing of silicon wafers. Furthermore, (3) it is desirable that the pulling rate be not increased in starting tail formation as compared with the pulling rate of the body in growing the above single crystal ingot. By taking these means, it is possible to produce epitaxial wafers having an almost constant, high level of gettering effect irrespective of the site of wafer slicing from the single crystal ingot and, furthermore, suppress the occurrence of defects
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 9.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing epitaxial wafers which comprises growing a single crystal silicon ingot while doping with not less than 1×10 13 atoms/cm 3 of nitrogen, slicing wafers from the thus-grown single crystal ingot, subjecting the wafers to 15 minutes to 4 hours of heat treatment at a temperature not lower than 700° C. but lower than 900° C. and subjecting the wafer surface after the above heat treatment to epitaxial growth treatment.
- Claim 2Depends on #1
A method of producing epitaxial wafers as claimed in claim 1 , wherein oxygen concentration in the wafers is not less than 11×10 17 atoms/cm 3 .
- Claim 3Depends on #1
A method of producing epitaxial wafers as claimed in claim 1 , wherein the 15-minutes to 4-hour heat treatment at a temperature not lower than 700° C. but lower than 900° C. is carried out prior to a s
Technical Overview & Description