Patents
US 6,709,930 B2#4503048 Most CitedExpiredUnited States (USPTO)Utility

Thicker oxide formation at the trench bottom by selective oxide deposition

19Forward Citations (#4503048 Global)
0.9/yrCitation Velocity (#8371418 Global)
3.70Citation PageRank (#5393599 Global)
21Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A trench MOSFET is formed by creating a trench in a semiconductor substrate, then forming a barrier layer over a portion of the side wall of the trench. A thick insulating layer is deposited in the bottom of the trench. The barrier layer is selected such that the thick insulating layer deposits in the bottom of the trench at a faster rate than the thick insulating layer deposits on the barrier layer. Embodiments of the present invention avoid stress and reliability problems associated with thermal growth of insulating layers, and avoid problems with control of the shape and thickness of the thick insulating layer encountered when a thick insulating layer is deposited, then etched to the proper shape and thickness.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 19.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a trench MOSFET, the method comprising: providing a semiconductor substrate; forming a trench in the substrate, the trench comprising a side wall and a bottom; forming a thin insulating layer overlying the side wall and the bottom of the trench; forming a barrier layer overlying the thin insulating layer on at least a portion of the side wall; etching the thin insulating layer to form an exposed portion of the semiconductor substrate in the bottom of the trench; and depositing a thick insulating layer overlying the bottom of the trench; wherein the barrier layer is sele

  2. Claim 2Depends on #1

    The method of claim 1

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 19 total)

PatentTitleYearCitations
CN 101,371,337 BTrench schottky barrier diode with differential oxide thickness20100
US 2006138535 A1Semiconductor device having trench gate structure and manufacturing method thereof—10
US 9,559,032 B2Method for forming MOS device passivation layer and MOS device20170
US 2015364397 A1Method for forming mos device passivation layer and mos device—1
US 10,727,318 B2Semiconductor device VDMOS having a gate insulating film having a high dielectric constant portion contacting the drift region for relaxing an electric field generated in the gate insulating film20201
US 8,143,655 B2Trench schottky barrier diode with differential oxide thickness20125
US 7,781,303 B2Method for preparing a shallow trench isolation20105
US 2008087896 A1Trench Schottky barrier diode with differential oxide thickness—25
US 6,800,509 B1Process for enhancement of voltage endurance and reduction of parasitic capacitance for a trench power MOSFET200444
US 2004203217 A1Bottom oxide formation process for preventing formation of voids in trench—9
US 2017092743 A1METHOD FOR PRODUCING A SEMICONDUCTOR POWER DEVICE (DMOS) INCLUDING GATE ELECTRODE FORMED OVER A GATE INSULATION FILM HAVING SiO2 PORTIONS AND A HIGH-K PORTION THEREBETWEEN—7
WO 2006/076298 A3Trench schottky barrier diode with differential oxide thickness—0
US 2005127465 A1Trench schottky barrier diode with differential oxide thickness—32
US 7,323,402 B2Trench Schottky barrier diode with differential oxide thickness200813
CN 101,866,849 BMethod for preparing oxide film at bottom of trench20120

Non-Patent Literature (1)

  • Pending U.S. application Ser. No. 10/180,154, filing date: Jun. 25, 2003.