US 6,709,807 B2#1834272 Most CitedExpiredUnited States (USPTO)Utility

Process for reducing edge roughness in patterned photoresist

34Forward Citations (#1834272 Global)
1.6/yrCitation Velocity (#3304381 Global)
6.01Citation PageRank (#2455707 Global)
11Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for reducing roughness from a surface of a patterned photoresist. The process includes exposing a substrate having the patterned photoresist thereon to a vapor, wherein the vapor penetrates into and/or reacts with the surface of the photoresist. The substrate having the patterned photoresist thereon is then heated to a temperature and for a time sufficient to cause the surface of the photoresist to flow and/or react with the vapor wherein the surface roughness decreases. Optionally, the substrate is exposed to radiation during the process to increase the etch resistance of the photoresist and/or facilitate the reaction of the vapor with the surface of the photoresist.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 34.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for reducing roughness from a surface of a patterned chemically amplified photoresist, the process comprising: a) exposing a substrate having patterned chemically amplified photoresist resulting from imaging and developing processing thereon to a vapor, wherein the vapor diffuses into the surface of the patterned photoresist; b) heating the substrate to a temperature and for a time sufficient to cause the surface of the patterned photoresist to flow wherein the surface roughness decreases; c) exposing the patterned photoresist to an activating radiation prior to, simultaneous with or

  2. Claim 2Independent Claim

    The process according to clai

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 34 total)

PatentTitleYearCitations
US 8,647,817 B2Vapor treatment process for pattern smoothing and inline critical dimension slimming20143
US 2008085612 A1Method to deposit conformal low temperature SiO2—30
US 8,932,793 B2Phenolic polymers and photoresists comprising same20152
DE 102004025837 A1Lithographic method for manufacture of resist pattern having line roughness involves unstructured exposure of resist to light e.g. floodlight of mercury vapor lamp and heating it so that its line roughness is reduced—0
WO 2015/069658 A1Method for using post-processing methods for accelerating euv lithography—3
US 7,151,040 B2Methods for increasing photo alignment margins200643
US 2009203216 A1Photolithographic systems and methods for producing sub-diffraction-limited features—9
US 8,848,161 B2Resist coating and developing apparatus, resist coating and developing method, resist-film processing apparatus, and resist-film processing method20140
US 2006046484 A1Method for integrated circuit fabrication using pitch multiplication—153
US 9,097,977 B2Process sequence for reducing pattern roughness and deformity20151
US 7,391,070 B2Semiconductor structures and memory device constructions20082
US 2008227031 A1Phenolic polymers and photoresists comprising same—11
US 2007131247 A1Method and apparatus for surface tension control in advanced photolithography—5
US 2013188158 A1Resist coating and developing apparatus, resist coating and developing method, resist-film processing apparatus, and resist-film processing method—0
US 7,098,105 B2Methods for forming semiconductor structures200625