US 6,709,770 B2#8093378 Most CitedExpiredUnited States (USPTO)Utility

Steel sheet hot dip coated with Zn-Al-Mg having high Al content

12Forward Citations (#8093378 Global)
0.6/yrCitation Velocity (#14494485 Global)
3.21Citation PageRank (#6784986 Global)
8Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A high Al hot-dip Zn—Al—Mg plated steel sheet is obtained by forming on a steel sheet surface a hot-dip plating layer comprising, in mass %, Al: more than 10 to 22% and Mg: 1-5%, and, optionally, Ti: 0.002-0.1%, B: 0.001-0.045% and Si: 0.005-0.5%. The plating layer exhibits a metallic structure of [primary crystal Al phase] mixed in a matrix of [Al/Zn/Zn 2 Mg ternary eutectic crystal structure]. Substantially no Zn 11 Mg 2 phase is present in the metallic structure of the plating layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 12.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A high Al hot-dip Zn—Al—Mg plated steel sheet obtained by forming on a steel sheet surface a hot-dip Zn-base plating layer of a composition comprising, in mass %, Al: more than 10 to 22%, Mg: 1-5%, Si: 0.005-0.5% and the balance of Zn and unavoidable impurities, which plating layer exhibits a metallic structure of primary crystal Al phase mixed in a matrix of Al/Zn/Zn 2 Mg ternary eutectic crystal structure.

  2. Claim 2Depends on #1

    A plated steel sheet according to claim 1 , wherein substantially no Zn 11 Mg 2 phase is present in the metallic structure of the plating layer.

  3. Claim 3Independent Claim

    A high Al hot-dip Zn—Al—Mg plated steel sheet obtained by forming on a steel sheet surface a hot-dip Zn-base plating layer of a composition comprising, in mass %, Al: more than 10 to 22%, Mg: 1-5%, Ti: 0.002-0.1%, B: 0.001-0.045%, Si: 0.005-0.5% and the ba

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (12 of 12 total)

PatentTitleYearCitations
US 9,771,636 B2Method of production of an aluminum plated steel sheet having excellent corrosion resistance with respect to alcohol or mixed gasoline of same and appearance20170
US 8,697,253 B2High-strength quenched formed body with good corrosion resistance20140
US 2011117382 A1High-strength quenched formed body with good corrosion resistance and process for producing the same—0
US 2018237897 A1Zn-Al-Mg COATED STEEL SHEET, AND METHOD OF PRODUCING Zn-Al-Mg COATED STEEL SHEET—13
US 8,962,153 B2Hot-dip Zn—Al alloy coated steel sheet and producing method therefor20155
US 2008131729 A1Highly corrosion-resistant hot-dip galvanized steel product excellent in surface smoothness and formability and process for producing same—2
US 7,998,533 B2Highly corrosion-resistant hot-dip galvanized steel product excellent in surface smoothness and formability and process for producing same20110
US 9,403,343 B2Aluminum plated steel sheet having excellent corrosion resistance with respect to alcohol or mixed gasoline of same and appearance20160
US 2014205857 A1Aluminum plated steel sheet having excellent corrosion resistance with respect to alcohol or mixed gasoline of same and appearance and method of production of same—6
US 2010086806 A1HOT-DIP Zn-Al ALLOY COATED STEEL SHEET AND PRODUCING METHOD THEREFOR—7
US 10,472,710 B2Zn—Al—Mg coated steel sheet, and method of producing Zn—Al—Mg coated steel sheet20191
US 11,618,938 B2Steel sheet having a hot-dip Zn—Al—Mg-based coating film excellent in terms of surface appearance and method of manufacturing the same20230

Non-Patent Literature (1)

  • D.J. Blickwede "55% Al-Zn-Alloy-Coated Sheet Steel" (Oct. 1979).