Process for making fiber mats for materials of construction having improved tear strength
Abstract
The invention relates to a coated fiber mat of improved tear strength upon dividing pieces of the coated mat and the coating which comprises a cured, non-woven, fiber glass mat containing a polysiloxane wherein the fibers are fixedly distributed in a formaldehyde type binder containing a binder modifier which is a crosslinked styrene/acrylic polymer, and to a process for the preparation of the mat.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 15.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
The process for making a cured polysiloxane containing non-woven fiber mat which comprises: (a) preparing an aqueous slurry of said fibers and removing excess water to form a wet fiber web; (b) separately preparing an aqueous dispersion or emulsion of a formaldehyde type binder containing between about 0.1 and about 20 wt. % of a crosslinkable styrene/(meth)acrylic polymer modifier for said binder; (c) adding between about 10 and about 40 wt. % , of (b), to (a); (d) adding a polysiloxane to said fiber web in an amount sufficient to provide a concentration of said polysiloxane in the mat of bet
- Claim 2Depends on #1
The process of claim 1 wherein the cured mat is subsequently coated o
Technical Overview & Description