Patents
US 6,703,337 B2#13321463 Most CitedExpiredUnited States (USPTO)Utility

Ceramic media

8Forward Citations (#13321463 Global)
0.4/yrCitation Velocity (#21881053 Global)
1.88Citation PageRank (#16055130 Global)
20Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Ceramic media made using ceramic components comprising from 5 to 60% by weight of spodumene and 95 to 40 wt % of other ceramic-forming components comprising clay and feldspar have a reduced tendency to shrink upon firing to form the media and improved physical properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Greenware for forming ceramic media comprising 5 to 20 wt. % of spodumene, and from 95 to 80 wt. % of other ceramic-forming components comprising from 50 to 95 wt. % of clay and from 5 to 50 wt. % of feldspar based on the combined weights of these ceramic-forming components, said ceramic-forming components being chosen, such that upon firing, said greenware forms said ceramic media and wherein said ceramic media has a linear shrinkage of less than 5% by comparison with the dimensions of the pre-fired greenware.

  2. Claim 2Depends on #1

    Greenware according to claim 1 in which the clay component has an MBI of from 11 to 13 meq/100 gm.

  3. Claim 3Depends on #1

    Greenware according to claim 1 in which the spodumene contains lithium in an amount, measured as lithium oxide, of from 7.25 to 7.75% by weight.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
GB 865,872 ALow thermal expansion ceramic body and a method of making it—6
US 3,228,779 ARefractory products and method of making19664
GB 1,023,471 AProcess for treating cellulosic fabric and product thereof—1
US 3,650,817 AMethod of manufacturing low thermal-expansion porcelain197211
US 3,818,087 AProcess of making thermal shack-resistant ceramic ware19746
US 3,979,216 ALow thermal expansion coefficient synthetic cordierite-containing ceramic bodies and method for producing same197631
US 4,098,725 ALow thermal expansive, electroconductive composite ceramics1978100
US 4,101,330 ALeucite-containing porcelains and method of making same197820
JP S56109869 AManufacture of low expansion ceramics—20
US 4,301,214 ALow thermal expansion ceramic and process198114
US 4,632,876 ACeramic spheroids having low density and high crush resistance1986163
JP H01115848 AProduction of glass ceramic—3
US 4,880,759 ABall clay slurry198936
CN 1,049,839 AHigh-alumina high-strength household porcelain and production method thereof—33
US 5,275,989 ACeramic composition for the production of the top layer of two-layered stoneware tiles199424
US 5,731,250 ACorrosion resistant ceramic bodies199812
US 5,773,103 AInorganic membranes using porous cordierite support199840
US 5,914,294 AAdsorptive monolith including activated carbon and method for making said monlith1999154
US 6,066,585 ACeramics having negative coefficient of thermal expansion, method of making such ceramics, and parts made from such ceramics200045
US 6,207,612 B1Removal of impurities from hydrocarbon streams200116

Non-Patent Literature (2)

  • Kusnik, et al., "Physical Properties of Spodumene-Kaolin Mixtures in the Firing Range 1270-1300 Degree", Materials Science Forum (1988), 34-36 (Int. Ceram. Conf., Austceram 88, Pt. 2), 931-5., (no month).
  • PCT Search Report (PCT/US02/13684) Aug. 2002.