Abstract

An improved flatting agent comprising an inorganic hydrogel having a pore volume of at least 1.0 ml/g, an average particle size in the range 1 to 10 microns, and a particle size distribution such that when the flatting agent is dispersed in a coating, the fineness of grind is at least 4.75 on the Hegman scale. The inorganic hydrogel flatting agents of this invention are prepared by milling an inorganic hydrogel under controlled temperature conditions wherein a volatiles content of at least 40 weight percent is maintained, to produce inorganic hydrogel particles characterized by a pore volume of at least 1.0 ml/g, an average particle size in the range of 1 to 10 microns, and a particle size distribution such that when the flatting agent is dispersed in a coating, the fineness of grind is at least 4.75 on the Hegman scale. Also provided in accordance with this invention are improved coating compositions comprising a full gloss coating containing the above described flatting agents dispersed in the full gloss coating in from 3 to 15 weight percent loading on a solids basis.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A flatting agent comprising an inorganic hydrogel having a pore volume of at least 1.0 ml/g, a volatiles content of at least 40 wt. % an average particle size in the range of 1 to 10 microns and a particle size distribution such that when the inorganic hydrogel flatting agent is dispersed in a coating vehicle, the fineness of grind is at least 4.75 on a Hegman scale.

  2. Claim 2Depends on #1

    The inorganic hydrogel flatting agent of claim 1 , wherein the average particle size is in the range 2 to 7 microns.

  3. Claim 3Depends on #1

    The inorganic hydrogel flatting agent of claim 1 , wherein the hydrogel is selected from silica, titania and alumina, or mixtures thereof.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

Non-Patent Literature (5)

  • "Gasil WP for Matting Clear Emulsion Based Wood Finishes" Joseph Crosfield & Sons Limited-Product Literature (No Date).
  • "New Advances in Fine Silica Technology" by S. E. Maskery presented at International Business Contact Club meeting-Mar. 24, 1976.
  • ASTM D 1210-79, "Standard Test Method for Fineness of Dispersion of Pigment-Vehicle Systems", pp. 220-233.
  • ASTM D 4438-85, "Standard Test Methods for Particle Size Distribution of Catalytic Material by Electronic Counting", pp. 1-4.
  • BS 3406: Part 5: 1983, "British Standard Methods for Determination of Particles Size of Powders".