Glass and glass powder mixture and use thereof for the production of a glass ceramic

6Forward Citations (#18413832 Global)
0.3/yrCitation Velocity (#27484666 Global)
1.43Citation PageRank (#24580553 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A glass or glass powder is fused from a starting mixture containing approximately 38 wt % to 48 wt % SO 2 , 15 wt % to 19 wt % Al 2 O 3 , 4.5 wt % to 11 wt % TiO 2 , 0 wt % to 1.5 wt % Na 2 O, 0 wt % to 1.5 wt % K 2 O and 23 wt % to 30 wt % CaO. In addition, a glass powder mixture includes two glass powders, a carbon black powder and an organic binder, the first glass powder having a mean particle size of approximately 150 μm to 250 μm, the second glass powder having a mean particle size of less than approximately 100 μm, which may be 10 μm to 70 μm. The glass or glass powder mixture is suitable for producing a glass ceramic, such as that used as a resistor seal and/or a gas-tight glass ceramic solder in a spark plug.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A glass comprising: a glass powder fused from a starting mixture including approximately 38 percent by weight to 48 percent by weight of SiO 2 , approximately 15 percent by weight to 19 percent by weight of Al 2 O 3 , approximately 4.5 percent by weight to 11 percent by weight of TiO 2 , and approximately 23 percent by weight to 30 percent by weight of CaO.

  2. Claim 2Depends on #1

    The glass of claim 1 , wherein the starting mixture includes at least one of alkali metal oxide, lithium oxide, potassium oxide, and sodium oxide, each one being in an amount up to approximately 1.5 percent by weight.

  3. Claim 3Depends on #1

    The glass of claim 1 , herein the starting mixture includes approximately 43 percent by weight to 48 percent by weight of the SiO 2 , approximately 16.5 percent by weight to 18 percent by weight of the Al 2 O 3 , approximately

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Duan, R, Effect of Changing Ti02 Content on Structure and Crystallization of CaO-A1203-SiO2 System Glasses, Journal of the European Ceramic Society, GB, Elsevier Science Publishers, Nov. 1, 1998, vol. 18, No. 12 (pp. 1729-1735) no month.
  • Villegas, MA, Propiedades Y Characterization Estructural De Vidrios Del Sistema CAO-TIO2-AL2O3-SIO2, Boletin De La Sociedad Espanola De Ceramica Y Vidrio, Madrid, 1995, vol. 34, No. 3 (pp. 135-139) no month.