Method of preparing copper metallization die for wirebonding
Abstract
A method of preparing a semiconductor wafer having a integrated circuits formed on it that have pads formed of copper includes the steps of removing oxide from the copper pads and then the vacuum packing the wafer in a shock-proof container. The oxide may be removed from the copper pads in a number of ways. A first way includes cleaning the wafer in an alkaline solution, performing acid neutralization on the cleaned wafer, and then drying the wafer. A second way includes cleaning the wafer with an acid solution, rinsing the acid cleaned wafer with water, applying an anti-oxidant activator to the surface of the copper pads, rinsing the wafer with water after the application of the anti-oxidant activator, and then drying the water rinsed wafer. Yet a third way includes plasma cleaning the copper pads using a combination of about 5-10% Hydrogen and about 90-95% Argon and then sputtering a very thin layer of aluminum on a surface of the copper pads. The layer of aluminum has a thickness of about 1-5 nanometers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 13.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of preparing a semiconductor wafer having a plurality of integrated circuits formed thereon, the integrated circuits having pads formed of copper, the method comprising the steps of: plasma cleaning the copper pads using about 5-10% Hydrogen and about 90-95% Argon; sputtering a very thin layer of a passivation material on a surface of the copper pads, said passivation layer having a thickness of about 1-5 nanometers; and vacuum packing the wafer in a shock proof container.
- Claim 2Depends on #1
The method of claim 1 , wherein the vacuum packing step comprises vacuum packing the wafer in a shock proof container.
- Claim 3Depends on #1
The method of claim 1 , wherein the passivation material comprises aluminum.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (13 of 13 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (3)
- Website for Small Precision Tools, "Copper Wire Ultra Fine Pitch Bonding-The Natural Progression in IC Assembly Technology?", Jurg Notzli et al. pp. 1-11.
- Website for Small Precision Tools, “Copper Wire Ultra Fine Pitch Bonding—The Natural Progression in IC Assembly Technology?”, Jurg Notzli et al. pp. 1-11.
- Website for The Nordic Electronics Packaging Guideline, "Chapter A: Wire Bonding", A1, pp. 1-4,A2 pp. 1-18, A4 pp. 1-8.