Water-soluble polymers with a water-soluble backbone and side units with a lower critical solution temperature, process for preparing them, aqueous compositions containing them and cosmetic use thereof
Abstract
Water-soluble polymers having a water-soluble backbone and side units having in water a lower critical solution temperature, LCST, the polymers being obtainable by free-radical precipitation polymerization of water-soluble monomers and of macromonomers comprising a unit with an LCST whose heat-induced demixing temperature in aqueous solution is from 5 to 40° C. for a concentration by mass in water of 1% of the said unit. Also described is a process for preparing these polymers by free-radical precipitation polymerization, and aqueous compositions containing these polymers and the use of these polymers and compositions, especially in cosmetics, for the cleansing and/or making up and/or care and/or antisun protection of keratin materials.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 18.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A water-soluble polymer comprising a water-soluble backbone and side units having in water a lower critical solution temperature, LCST, the polymer being obtainable by free-radical precipitation polymerization of: a) one or more water-soluble monomers (Ia) and, optionally, of one or more hydrophobic monomers (Ib) in a smaller amount relative to the monomer(s) (Ia), the monomers (Ia) and (Ib) bearing at least one unsaturated function that can be polymerized to form the water-soluble backbone; b) one or more macromonomers corresponding to formula (II): A—X—B (II), in which A is a group comprisi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 18 total)
References Cited — Backward Prior Art (13)
Non-Patent Literature (5)
- D. Hourdet, et al., Polymer, vol. 35, No. 12, pp. 2624-2630, "Reversible Thermothickening of Aqueous Polymer Solutions", 1994.
- D. Hourdet, et al., Polymer, vol. 38, No. 10, pp. 2535-2547, XP-004059755, "Synthesis of Thermoassociative Copolymers", May 1, 1997.
- F. E. Bailey, Jr., et al., Journal of Applied Polymer Science, vol. 1, No. 1, pp. 56-62, "Some Properties of Poly(Ethylene Oxide)<1 >in Aqueous Solution", 1959.
- F. E. Bailey, Jr., et al., Journal of Applied Polymer Science, vol. 1, No. 1, pp. 56-62, "Some Properties of Poly(Ethylene Oxide)1 in Aqueous Solution", 1959.
- F. L'Alloret, et al., Coll. Polym. Sci., vol. 273, No. 12, pp. 1163-1173, "Aqueous Solution Behavior of New Thermoassociative Polymers", 1995.