Composition for controlling spangle size, a coated steel product, and a coating method
Abstract
A method of coating of steel products such as plate and sheet using an aluminum-zinc coating alloy includes modifying the coating bath with a particulate compound constituent in effective amounts to control the spangle facet size of the coated product, improve tension bend rust stain performance, and improve coated product paintability. Constituents include borides such as titanium boride and aluminum borides, carbides such as titanium carbide, and aluminides such as titanium aluminide. The method produces a coated steel product that does not require temper rolling for painting.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 8.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a method of coating a steel product using a molten aluminum-zinc alloy bath, the improvement comprising modifying the composition of the aluminum-zinc alloy by adding an effective amount of one or more of a particulate compound constituent that produces a coated spangle size on a substrate of between about 400 to 500 microns, said grain refining particulate compound selected from the group consisting of boride compounds in an amount between about 0.0008 to 0.0012% by weight, and having one of titanium and aluminum.
- Claim 2Depends on #1
The method of claim 1 , wherein the particulate compound constitute is one of TiB 2 , AlB 2 , and AlB 12 .
- Claim 3Depends on #1
The method of claim 1 , wherein a particle size of the particulate compound constituent ranges between about 0.01 microns and about 25 microns.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (5)
- International Materials Reviews, vol. 34,No. 5, Grain Refining of Aluminum and its Alloys Using Inoculants, pp 247-260, D. G. McCartney (1989) (no month given).
- Journal of the Institute of Metals, 1951-52, vol. 80, "The Grain Refinement of Aluminum Alloy Castings by Additions of Titanium and Boron," A. Cibula, et al., pp. 1-16 (no month given).
- Metallurgical Transactions, vol. 18A, Apr. 1987, "The Role of Boron inthe Grain Refinment of Aluminum with Titanium," M. M. Guzowski, et al., pp. 603-619.
- Metallurgical Transactions, vol. 2, Feb. 1971 "Grain Refinement in Aluminum Alloyed with Titanium and Boron," J. A. Marcantonio, et al., pp. 465-471.
- Metallurgical Transactions, vol. 7b, Jun. 1976, "Factors Affecting the Grain-Refinement of Aluminum Using Titanium and Boron," G. P. Jones, et al., pp. 223-234.