Process for producing a fiber-reinforced thermoplastic resin molded product and product thereby produced
Abstract
A new process for producing a fiber-reinforced thermoplastic resin molded product with a high mechanical strength and no heat substantial deterioration of the resin, by an efficient heating without applying shear stress to the fiber-reinforced thermoplastic resin base material and a molded product, for example, a tiptoe core for a safety shoe produced by said process are provided.The fiber-reinforced thermoplastic resin base material P1 in a string form or a tape form is scattered and accumulated in a vessel such as tube 11, and a heating gas passed to the accumulated base material to melt heat, and preferably press by a plunger 15, the base material P1, whereby a molten mass P2 is formed, and then the molten mass P2 is dislocated to a mold to be press-mold. Said base material preferably satisfies the following formula: {fraction (1/100<=RHO1/rho0<=½, wherein rho0 means a density where said base material is scattered and accumulated and rho0 means a true density of said base material.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 5.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for producing a fiber-reinforced thermoplastic resin molded product, which comprises a step of supplying a base material wherein a fiber-reinforced thermoplastic resin base material in a string form or in a tape form is scattered and accumulated, a step of forming a molten mass wherein a heating gas is passed through said base material accumulated to heat-melt it thereby to form a molten mass, and a molding step wherein said molten mass is supplied to a mold and then is press-molded to form a molded product.
- Claim 2Depends on #1
The process for producing a fiber-reinforced thermoplastic resin molded product according to claim 1 , wherein said base material satisfies the following formula: {fraction (1/100)}ρ 1 /ρ 0 ½, wherein ρ 1 is the density of said base material which is scattered and accumulated and ρ 0 is the true density of said
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗