The present invention relates to a method for treating spent tin or tin/lead stripping solution used in the electronic industry, particularly in the manufacture of printed circuit boards or a lead frames. Said method comprises (i) electrolytically reducing copper ions in the solution to copper at a low temperature; (ii) electrolytically oxidizing Sn 2+ and Pb 2+ in the solution at a high temperature to form solid tin and lead oxides and hydroxides; (iii) separating solid tin and lead oxides and hydroxides from the solution; (iv) dissolving tin and lead oxides and hydroxides obtained in step (iii) in a strong alkali or acidic solution; and (v) electrolytically reducing the alkali or acidic solution obtained in step (iv) at a high temperature to recover metallic tin and lead. Also, the filtrate obtained in step (iii) above is useful for preparing fresh tin or tin/lead stripping solution.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for treating spent tin or tin/lead stripping solution, comprising: (i) electrolytically reducing copper ions in the solution to copper at a low temperature; (ii) electrolytically oxidizing Sn 2+ and Pb 2+ in the solution at a high temperature to form solid tin and lead oxides and hydroxides; (iii) separating solid tin and lead oxides and hydroxides from the solution; (iv) dissolving tin and lead oxides and hydroxides obtained in step (iii) in a strong alkali or acidic solution; and (v) electrolytically reducing the alkali or acidic solution obtained in step (iv) at a high temperatur

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein during step (i), the electrolytic reduction is conducted at a temperature of about −5° C. to about 40° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (1)