Abstract

A method for protecting low-carbon steel and stainless steel from coking and corrosion at elevated temperatures in corrosive environments, such as during ethylene production by pyrolysis of hydrocarbons or the reduction of oxide ores, by coating the stainless steel with a coating of MCrAlXSiT in which M is nickel, cobalt, iron or a mixture thereof, X is yttrium, hafnium, zirconium, lanthanum, scandium or combination thereof, and T is tantalum, titanium, platinum, palladium, rhenium, molybdenum, tungsten, niobium, boron or combination thereof. A blended powder composition to produce a desired MCrAlXSiT surface alloy may be applied to the substrate. The overlay coating and stainless steel substrate preferably are heat-treated at about 1000 to 1200° C. for about 10 minutes or longer effective to metallurgically bond the overlay coating to the substrate and to form a multiphased microstructure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 31.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for providing a protective and inert coating on carbon steel and stainless steel comprising depositing onto a carbon steel or stainless steel substrate and metallurgically bonding thereto by reactive sintering a continuous coating of a MCrAlXSi alloy, where M=nickel, cobalt or iron or mixture thereof and X=yttrium, hafnium, zirconium, lanthanum, scandium or combination thereof, having about 10 to 40 wt % chromium, about 1 to 25 wt % aluminum, about 1 to about 40 wt % silicon and 0.25 to about 5 wt % X, the balance at least 40 wt % M.

  2. Claim 2Depends on #1

    A method as claimed in claim 1 in which the coating is deposited by physical vapour deposition, thermal spray, plasma transferred arc, isostatic pressing or by slurry coating.

  3. Claim 3Depends on #1

    A method as claimed in claim 1 , in which the MCrAlXSi additionally comprises 0.1 to abo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • "Processing and Properties of Materials" entitled "The Effect of Time at Temperature on Silicon-Titanium Diffusion Coating on IN738 Base Alloy" by M.C. Meelu and M.H. Lorretto, p. 1241-1246, no date.