Herein disclosed is surface-modified nickel fine powder in which a precursor of barium titanate having a perovskite structure and consisting of a reaction product of a soluble titanium-containing compound and a soluble barium-containing compound is adhered to the surface of individual nickel fine particles, wherein the fine powder shows X-ray diffraction peaks of nickel and is free of any peak of barium titanate having a perovskite structure in the X-ray diffraction pattern determined by the X-ray diffraction method, but the fine powder shows X-ray diffraction peaks of both nickel and barium titanate having a perovskite structure in the X-ray diffraction pattern after the fine powder is subjected to a heat-treatment at a temperature of not less than 400° C. The nickel fine powder has a small heat shrinkage factor upon firing and improved resistance to oxidation. The powder permits the inhibition of any such phenomenon that nickel is oxidized and the oxidized nickel penetrates into a ceramic dielectric material during firing. The powder is suitable for use as a material for a conductive paste and, in particular, for forming a conductive paste used in making a multilayer ceramic capa

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for preparing nickel fine powder surface-modified with a precursor comprising the steps of bringing nickel fine particles into contact with a solution containing a combination of a soluble titanium-containing compound and a soluble barium-containing compound, which can form barium titanate having a perovskite structure through a heat-treatment at a temperature of not less than 400° C to thus adhere, to the surface of the individual nickel fine particles, a precursor consisting of the reaction product of the soluble titanium-containing compound and the soluble barium-containing compoun

  2. Claim 2Depends on #1

    The method as set forth in claim 1 , wherein the precursor is adhered to the surface of the individual nickel fine particles, dried and then heat-treated at a temperature of less than 400° C.