Postweld heat treatment process of carbon steel and low alloy steel

17Forward Citations (#5337276 Global)
0.8/yrCitation Velocity (#9700903 Global)
2.89Citation PageRank (#8029616 Global)
0Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The creep strength of a welded joint portion is improved, and damage of the welded joint portion based on the generation or development of cracks is suppressed. A postweld heat treatment process, wherein a welded joint made of carbon steel and low alloy steel is held within austenite single-phase temperature range for a given time and subsequently the joint is cooled by air-cooling or by slow cooling at a cooling rate lower than that of the air-cooling.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 17.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A postweld heat treatment process comprising the steps of holding a welded joint made of carbon steel or low alloy steel within austenite single-phase temperature range for a given time, thereby annealing the joint, and subsequently cooling the joint by air-cooling or by slow cooling at a cooling rate lower than that of the air-cooling.

  2. Claim 2Depends on #1

    The postweld heat treatment process according to claim 1 , wherein the joint is held at 930° C. within the austenite single-phase temperature range for 30 minutes and is cooled by furnace cooling.

  3. Claim 3Depends on #1

    The postweld heat treatment process according to claim 1 , wherein the cooling rate upon the furnace cooling is set to 1° C. per minute.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 17 total)

PatentTitleYearCitations
US 10,173,281 B2Bonded structure of dissimilar metallic materials and method of joining dissimilar metallic materials20192
US 2009120535 A1Method of bonding steel members, method of enhancing bonding strength of united body formed of steel members, steel product, and die-cast product—0
US 2014144889 A1Bonded Structure of Dissimilar Metallic Materials and Method of Joining Dissimilar Metallic Materials—7
WO 2008/031210 A1Method for manufacturing a welded assembly—7
US 7,475,478 B2Method for manufacturing automotive structural members200914
US 7,340,378 B1Weighted event counting system and method for processor performance measurements200831
US 2008115863 A1Method for improving the performance of seam-welded joints using post-weld heat treatment—20
US 2023041257 A1Method to determine post-weld heat treatment requirements for external welded attachment to avoid environmental stress corrosion cracking—0
US 2007045384 A1Method for manufacturing gas and liquid storage tanks—5
US 2007034673 A1Seam-welded air hardenable steel constructions—1
US 7,232,053 B2Seam-welded air hardenable steel constructions20075
US 2009056223 A1Quench ring rim and methods for fabricating—1
US 11,965,819 B2Method to determine post-weld heat treatment requirements for external welded attachment to avoid environmental stress corrosion cracking20240
US 7,618,503 B2Method for improving the performance of seam-welded joints using post-weld heat treatment200911
US 7,926,180 B2Method for manufacturing gas and liquid storage tanks20111

References Cited — Backward Prior Art (0)

No backward patent references recorded.

Non-Patent Literature (5)

  • Kimura, K., et al. "Effect of Initial Microstructure on Inherent Creep Strength of Ferritic Steels", Current Advances in Materials and Processes, The Iron and Steel Institute of Japan, vol. 12, No. 6 (1999), p. 1317.
  • Kimura, K., et al. "Effect of Initial Microstructure on Long Term Creep Strength of a Low Alloy Ferritic Steel", Iron and Steel, The Iron and Steel Institute of Japan, vol. 86, No. 8 (2000), pp. 44-51.
  • Kimura, K., et al. "Effect of Initial Microstructure on the Long Term Creep Strength of a Low Alloy Cr-Mo Steel", Parsons 2000 Advanced Materials for 21<st >Century Turbines and Power Plant, The Institute of Materials, London, U.K., 1997, pp. 558-571.
  • Kimura, K., et al. "Effect of Initial Microstructure on the Long Term Creep Strength of a Low Alloy Cr-Mo Steel", Parsons 2000 Advanced Materials for 21st Century Turbines and Power Plant, The Institute of Materials, London, U.K., 1997, pp. 558-571.
  • Kimura, K., et al. "Improvement in Creep Strength of Welded Joint of 2.25Cr-1Mo Steel by PWHT", Current Advances in Materials and Processes, The Iron and Steel Institute of Japan, vol. 14, No. 3 (2001), p. 659.