Production of thin steel strip
Abstract
A plain carbon steel strip is continuously cast in a twin roll caster and passes to a run out table on which it is subjected to accelerated cooling by means of cooling headers whereby it is cooled to transform the strip from austenite to ferrite at a temperature range between 850° C. and 400° C. at a cooling rate of not less than 90° C./sec, such that the strip has a yield strength of greater than 450 MPa. The strip after casting and before cooling is passed through a hot rolling mill to reduce the thickness of strip by at least 15% and up to 50%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 0.
Claims (10)
- Claim 1Independent Claim
A method of producing steel strip comprising: supporting a casting pool of molten low carbon steel on a pair of chilled casting rolls forming a nip between them and continuously casting solidified strip of no more than 5 mm in thickness and including austenite grains by rotating the rolls in mutually opposite directions such that the solidified strip moves downwardly from the nip; passing the strip through a rolling mill in which the strip is hot rolled to produce a reduction in the strip thickness of at least 15%; and cooling the strip to transform the austenite to ferrite within a temperature range between 850° C. and 400° C. at a cooling rate of more than 100° C./sec.
- Claim 2Depends on #1
A method as claimed in claim 1 , wherein said cooling rate is in the range 100° C./sec to 300° C./sec.
- Claim 3Depends on #1
A method as claimed in claim 1 , wherein the low carbon steel is a siliconlmanganese killed steel having the following composition by weight: Carbon 0.02-0.08% Manganese 0.30-0.80% Silicon 0.10-0.40% Sulphur 0.002-0.05% Aluminum less than 0.01%
- Claim 4Depends on #1
A method as claimed in claim 1 , wherein the low carbon steel is aluminum killed steel.
- Claim 5Depends on #4
A method as claimed in claim 4 , wherein the aluminum killed steel has the following composition by weight: Carbon 0.02-0.08% Manganese 0.40% max Silicon 0.05% max Sulphur 0.002-0.05% Aluminum 0.05% max
- Claim 6Depends on #1
A method as claimed in claim 1 , wherein the finished strip has a yield strength of greater than 450 MPa.
- Claim 7Depends on #1
A method as claimed in claim 1 , wherein said cooling rate is in the range 100° C./sec to 300° C./sec and the strip has a yield strength of at least 450 Mpa.
- Claim 8Depends on #7
A method as claimed in claim 7 , wherein the strip has a yield strength in the range of 450 MPa to 700 Mpa.
- Claim 9Depends on #1
A method as claimed in claim 1 , wherein the low carbon steel is a silicon/manganese killed steel, and the strip is cooled at a cooling rate in the range of 100° C./sec to 300° C./sec to produce a strip having a yield strength of at least 450 MPa.
- Claim 10Depends on #9
A method as claimed in claim 9 , wherein the final strip has a yield strength i
Technical Overview & Description
This application claims priority to U.S. Provisional Application Ser. No. 60/270,861, filed Feb. 26, 2001, and to U.S. Provisional Application Ser. No. 60/236,389, filed Sep. 29, 2000. BACKGROUND AND SUMMARY OF THE INVENTION This invention relates to the production of thin steel strip in a strip caster, particularly a twin roll caster. In a twin roll caster, molten metal is introduced between a pair of contra-rotated horizontal casting rolls which are cooled so that metal shells solidify on the moving roll surfaces and are brought together at the nip between them to produce a solidified strip product delivered downwardly from the nip between the rolls. The term “nip” is used herein to refer to the general region at which the rolls are closest together. The molten metal may be poured from a ladle into a smaller vessel from which it flows through a metal delivery nozzle located above the nip so as to direct it into the nip between the rolls, so forming a casting pool of molten metal supported on the casting surfaces of the rolls immediately above the nip and extending along the length of the nip. This casting pool is usually confined between side plates or dams held in sliding engagement with end surfaces of the rolls so as to dam the two ends of the casting pool against outflow, although alternative means such as electromagnetic barriers have also been proposed. When casting steel strip in a twin roll caster the strip leaves the nip at very high temperatures of the order of 1400° C. and if exposed to air, it suffers very rapid scaling due to oxidation at such high temperatures. It has therefore been proposed to shroud the newly cast strip within an enclosure containing a non-oxidising atmosphere until its temperature has been reduced significantly, typically to a temperature of the order of 1200° C. or less so as to reduce scaling. One such proposal is described in U.S. Pat. No. 5,762,126 according to which the cast strip is pa
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|