Method for high deposition rate solder electroplating on a microelectronic workpiece
Abstract
The present invention is directed to an improved electroplating method, chemistry, and apparatus for selectively depositing tin/lead solder bumps and other structures at a high deposition rate pursuant to manufacturing a microelectronic device from a workpiece, such as a semiconductor wafer. An apparatus for plating solder on a microelectronic workpiece in accordance with one aspect of the present invention comprises a reactor chamber containing an electroplating solution having free ions of tin and lead for plating onto the workpiece. A chemical delivery system is used to deliver the electroplating solution to the reactor chamber at a high flow rate. A workpiece support is used that includes a contact assembly for providing electroplating power to a surface at a side of the workpiece that is to be plated. The contact contacts the workpiece at a large plurality of discrete contact points that isolated from exposure to the electroplating solution. An anode, preferably a consumable anode, is spaced from the workpiece support within the reaction chamber and is in contact with the electroplating solution. In accordance with one embodiment the electroplating solution comprises a concent
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for electroplating a tin/lead solder onto a surface of a microelectronic workpiece, comprising: exposing the surface of the microelectronic workpiece to a plating solution including a source of tin ions and a source of lead ions; placing an electrode in contact with the plating solution; and applying current between the workpiece and the electrode to electrolytically deposit a tin/lead solder on the surface of the workpiece at a deposition rate of at least 2 microns per minute.
- Claim 2Depends on #1
The method of claim 1 , wherein the tin/lead solder is deposited at a rate of at least 2 to 8 microns per minute.
- Claim 3Depends on #2
The method of claim 2 , wherein the tin/lead solder is deposited at a rate of 4 to 8 microns per minute.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2012252203 A1 | Controlled electroplated solder bumps | — | 0 |
| US 8,741,765 B2 | Controlled electroplated solder bumps | 2014 | 0 |