A substrate with a metal oxide film deposited thereon is annealed, and then the surface of the metal oxide film is exposed to a plasma, after which the metal oxide film is removed by wet-etching.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 75.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A wet-etching method, comprising: a first step of annealing a substrate with a metal oxide film deposited thereon; a second step of exposing a surface of the annealed metal oxide film to a plasma; and a third step of removing, by wet-etching, at least a surface portion of the metal oxide film, which has been exposed to the plasma.

  2. Claim 2Depends on #1

    The wet-etching method of claim 1 , wherein the second step includes a step of applying a bias power to the substrate.

  3. Claim 3Depends on #1

    The wet-etching method of claim 1 , wherein the plasma is a plasma made of an HBr-containing gas.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 75 total)

Non-Patent Literature (1)

  • J.J. Chambers et al. "Effect of Composition and Post-Deposition Annealing on the Etch Rate of Hafnium and Zirconium Silicates in Dilute HF", Texas Instruments Incorporated Sep. 2001.