Patents
US 6,663,753 B2#917099 Most CitedExpiredUnited States (USPTO)Utility

Method of making coated article including DLC inclusive layer over low-E coating

51Forward Citations (#917099 Global)
2.2/yrCitation Velocity (#1673493 Global)
3.10Citation PageRank (#7201009 Global)
50Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A substrate is coated with a low-E coating system including at least one infrared (IR) reflective layer. A diamond-like carbon (DLC) inclusive protective coating system (e.g., including at least one highly tetrahedral amorphous carbon (ta-C) inclusive layer having sp 3 carbon—carbon bonds) is provided on the substrate over at least the IR reflective layer in order to make the low-E coating system scratch resistant, abrasion resistant, and generally mechanically durable. The DLC inclusive protective coating system may be hydrophobic, hydrophillic, or neutral in different embodiments of the invention. Optionally, at least one fluoro-alkyl silane (FAS) compound inclusive layer may be provided on the substrate over at least one of the DLC inclusive layer(s) in hydrophobic embodiments in order to increase contact angle θ of the coated article.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 51.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of making a coated article, the method comprising the steps of: providing a substrate; depositing a low-E layer arrangement including at least one IR reflecting layer on the substrate; depositing a DLC inclusive layer on the substrate over the low-E layer arrangement in a manner such that the substrate and the IR reflecting layer are maintained at temperature(s) no greater than about 200 degrees C. during said depositing of the DLC inclusive layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said depositing the DLC inclusive layer on the substrate over the low-E layer arrangement is performed in a manner such that the substrate and the IR reflecting layer are maintained at temperature(s) no greater than about 125 degrees C. during said depositing of the DLC inclusive layer.

  3. Claim 3Independent Claim

    The me

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "6001 Chemical Abstracts", Columbus, Ohio (1996) 1pg.
  • "ANSIZ26.1". Society of Automotive Engineers. American National Standards Institute. Inc., 1977.
  • "Deposition of Carbon Films by a Filtered Cathodic Arc", Kuhn et al., Jan. 1993, pp. 1350-1354.
  • "Electronic Density of States in Highly Tetrahedral Amorphous Carbon", Veerasamy et al., Aug. 1993, pp. 319-326.
  • "Highly Tetrahedral, Diamond-like Amorphous Hydrogenated Carbon Prepared From a Plasma Beam Source", Sattel et al., Published Feb. 1994 pp. 2797-2799.