US 6,660,135 B2#13830965 Most CitedExpiredUnited States (USPTO)Utility

Staged aluminum deposition process for filling vias

8Forward Citations (#13830965 Global)
0.3/yrCitation Velocity (#22438924 Global)
1.56Citation PageRank (#21594901 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A semiconductor metallization process for providing complete via fill on a substrate, free of voids, and a planar metal surface, free of grooves. In one aspect, a refractory layer is deposited onto a substrate having high aspect ratio contacts or vias formed thereon. A conformal PVD metal layer, such as Al or Cu, is then deposited onto the refractory layer at a pressure below about 1 milliTorr. The vias and/or contacts are then filled with metal, such as by reflowing additional metal deposited by physical vapor deposition on the conformal PVD metal layer. The process is preferably performed in an integrated processing system that includes a long throw PVD chamber, wherein a target and a substrate are separated by at least 100 mm, and a hot metal PVD chamber, also serving as a reflow chamber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a feature on a substrate, comprising: a) depositing a barrier/wetting layer over the surfaces of an aperture in the substrate; b) physical vapor depositing a conformal first metal layer over the surface of the barrier/wetting layer without capping or filling the aperture at a chamber pressure less than about 1 milliTorr; and c) physical vapor depositing a second metal layer on the conformal first metal layer at a temperature below about 350° C.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising reflowing the second metal layer.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the second metal layer is reflowed at a temperature less than about 500° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • G. Yao et al . "Advanced Aluminum Planarization Solutions for Sub 0.25 mum Technologies," Technical Symposium, Semicon Korea, 1999.
  • G. Yao et al . “Advanced Aluminum Planarization Solutions for Sub 0.25 μm Technologies,” Technical Symposium, Semicon Korea, 1999.
  • G. Yao et al., "Advanced Warm Aluminum for 0.25 mum Plug Filling," Conference Proceedings ULSI XIII, pp. 243-249, 1998.
  • G. Yao et al., “Advanced Warm Aluminum for 0.25 μm Plug Filling,” Conference Proceedings ULSI XIII, pp. 243-249, 1998.
  • Search report for EP SN 00113013.7.