Fe-Ni based permalloy and method of producing the same and cast slab
Abstract
A Fe-Ni based permalloy comprises Ni: 30-85 wt %, C: not more than 0.015 wt %, Si: not more than 1.0 wt %, Mn: not more than 1.0 wt %, P: not more than 0.01 wt %, S: not more than 0.005 wt %, O: not more than 0.0060 wt %, Al: not more than 0.02 wt % and, if necessary, not more than 15 wt % of at least one selected from the group consisting of Mo, Cu, Co and Nb within a range of not more than 20 wt % in total.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 7.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A Fe—Ni based permalloy comprising Ni: 35-40 wt %, C: not more than 0.015 wt %, Si: not more than 1.0 wt %, Mn: not more than 1.0 wt %, P: not more than 0.01 wt %, S: not more than 0.005 wt %, O: not more than 0.006 wt %, Al: not more than 0.02 wt % and the remainder being Fe and inevitable impurities, and having such magnetic properties that a maximum magnetic permeability μm is not less than 50000, an initial magnetic permeability μi is not less than 10000 and a coercive force Hc is not more than 0.05 (Oe), provided that Ni segregation amount C Ni s represented by the following equation is n
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (4)
- English Language Abstract of JP 2000-73108.
- English Language Abstract of JP 2620353.
- English Language Abstract of JP 60-2651.
- English Language Abstract of JP 62-142749.