Method of manufacturing electrode or electrode-electrolyte membrane joint body for fuel cell and electrode for fuel cell
Abstract
A paste-like ink is prepared by dissolving camphor in an alcoholic solvent and dispersing fine carbon particles with a catalyst carried thereon in the solvent (step S100). A sheet-like electrode-forming member is formed on an electrolyte membrane by screen printing the paste-like ink thus obtained (step S102). The electrode-forming member is dried at 80° C. for one hour, in order to deposit camphor included in the electrode-forming member as a pore-forming agent (step S104). The electrode-forming member and the electrolyte membrane are joined with each other by hot pressing (step S106). The joint body of the electrode-forming member and the electrolyte membrane is dried under vacuum at 80° C. for three hours, in order to sublimate and remove camphor depositing in the electrode-forming member (step S108). This gives an electricity-generating layer that is a joint body of an electrode having a plurality of pores and the electrolyte membrane. The manufacturing process of the invention thus gives a joint body of an electrode having sufficient gas permeability and electrical conductivity and an electrolyte membrane.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 5.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of manufacturing an electrode for a fuel cell, said electrode having a plurality of pores and comprising carbon particles with a catalyst carried thereon, said method comprising: (a) preparing an electrode-forming member comprising said carbon particles by: (a1) dissolving said pore-forming agent that can be sublimed into a solvent that allows dissolution of said pore-forming agent and dispersing said carbon particles in the solvent, so as to prepare a mixture; (a2) forming the mixture into a predetermined shape of said electrode-forming member; and (a3) drying the mixture formed into
- Claim 2Depends on #1
A method in accordance with claim 1 , wherein said steps (a1) and (
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (21)
Non-Patent Literature (5)
- Abstract Number 108:115868 (w/Patent Abstracts of Japan Publication Number 62281272, Publication Date of Dec. 7, 1987).
- Abstract Number 108:2243422 (w/Patent Abstracts of Japan Publication Number 63048752, Publication Date of Mar. 1, 1988).
- Abstract Number 122:35176 (w/Patent Abstracts of Japan Publication Number 06267545, Publication Date of Sep. 22, 1994).
- Abstract Number 125:200820 (w/Patent Abstracts of Japan Publication Number 08185865, Publication Date of Jul. 16, 1996).
- Abstract Number 125:200822 (w/Patent Abstracts of Japan, Publication Number 08185867, Publication Date of Jul. 16, 1996).