Patents
US 6,649,502 B2#60299317 Most CitedExpiredUnited States (USPTO)Utility

Methods of forming multilayer dielectric regions using varied deposition parameters

1Forward Citations (#60299317 Global)
0.0/yrCitation Velocity (#56749834 Global)
0.76Citation PageRank (#60299317 Global)
2Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A dielectric region for a device such as a memory cell capacitor is formed by depositing a metal oxide, such as tantalum oxide, on a substrate at a first deposition rate in a first atmosphere maintained within a first temperature range and a first pressure range that produce a first tantalum oxide layer with a desirable step coverage. Metal oxide is subsequently deposited on the first metal oxide layer in a second atmosphere maintained within a second temperature range and a second pressure range that produce a second deposition rate greater than the first deposition rate to form a second tantalum oxide layer on the first tantalum oxide layer. For example, the first atmosphere may be maintained at a temperature in a range from about 350° C. to about 460° C. and a pressure in a range from about 0.01 Torr to about 2.0 Torr during formation of a first tantalum oxide layer, and the second atmosphere may be maintained at a temperature in a range from about 400° C. to about 500° C. and a pressure in a range from about 0.1 Torr to about 10.0 Torr during formation of a second tantalum oxide layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming a dielectric region, the method comprising: depositing tantalum oxide on a substrate to a thickness of about 1 Å or greater in an atmosphere having a temperature in a range from about 350° C. to about 460° C. and a first pressure to form a first tantalum oxide layer; and depositing tantalum oxide on the first tantalum oxide layer to a thickness of about 30 Å or greater in an atmosphere having a temperature in a range from about 400° C. to about 500° C. and a second pressure greater that the first pressure to form a second tantalum oxide layer on the first tantalum oxide lay

  2. Claim 2Depends on #1

    A method according to claim 1 : wherein depositing tantalum oxide on a substrate comprises depositing tantalum oxide on the substrate to a thickness of about 10 Å or greater in an atmosphere having a temperat