Patents
US 6,645,778 B2#29099129 Most CitedExpiredUnited States (USPTO)Utility

Method for the preparation of ferroelectric semiconductive coating and apparatus for removing environmental air pollutants using this coating and electric power

3Forward Citations (#29099129 Global)
0.1/yrCitation Velocity (#41170523 Global)
1.36Citation PageRank (#26692312 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed is a method for preparing ferroelectric semiconductive coatings which is capable of coating the ferroelectric semiconductor onto a metal and forming electron-hole pairs on the surface of the ferroelectric semiconductor by using 440 V and 30K˜100K Hz alternating current electric energy of a high voltage and a high frequency as an energy source, based upon an energy level difference between the semiconductor and the metal, whereby it can exhibit an effective surface reaction in the range of the oxidation and reduction reaction even in the closed space where no ultraviolet irradiation occurs.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a ferroelectric semiconductive coating, comprising the steps of: (a) mixing tetraethyl orthotitanate with a water/alkoxide mixture in a molar ratio of between 10-50 to form a mixture, stirring the mixture for about 2-8 hours to decompose the mixture, and adding a water solution of 1 to 7 wt. % hydrochloric acid or sulfuric acid to the decomposed mixture to form titanic acid oxide; (b) mixing the titanic acid oxide produced in step (a) with a methanol solution, adding an oxygen producing activating agent containing about 0.1-0.7 mole % manganese in 12.5 wt. % manganese ch

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗