Method of making coated article including layer(s) of diamond-like carbon which may be hydrophobic

20Forward Citations (#4314546 Global)
0.9/yrCitation Velocity (#8333651 Global)
2.50Citation PageRank (#10157916 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process includes coating a substrate with a hydrophobic coating system including highly tetrahedral amorphous carbon that is a form of diamond-like carbon (DLC). In certain embodiments, the coating system is deposited on the substrate in a manner to increase its hydrophobicity. In certain embodiments, the coating system is deposited in a manner such that it has an average hardness of at least about 10 GPa, more preferably from about 20-80 GPa. In certain embodiments, the coating system includes first and second DLC inclusive layers that are deposited using one or more ion beam deposition devices, wherein different gases are used to deposit the respective DLC inclusive layers such that the overlying layer has greater scratch resistance characteristics than the underlying layer which functions as an anchoring layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of making a coated article, the method comprising: providing a substrate; depositing a first DLC inclusive layer on the substrate using a first gas including silicon (Si); and depositing a second DLC inclusive layer on the substrate and on the first DLC inclusive layer using a second gas different than the first gas so that the resulting article has an initial contact angle θ of at least about 80 degrees.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising depositing the second layer so as to include ta-C and so that the resulting article has an initial contact angle θ of at least about 100 degrees, and wherein said depositing steps are performed using ion beam deposition.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein said first gas includes a silane compound and said second gas includes a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "6001 Chemical Abstracts", Columbus, Ohio (1996) 1pg.
  • "ANSI Z26.1", Society of Automotive Engineers, American National Standards Institute, Inc., 1977, No Page Numbers.
  • "Deposition of Carbon Films by a Filtered Cathodic Arc", Kuhn et al., Jan. 1993, pp. 1350-1354.
  • "Electronic Density of States in Highly Tetrahedral Amorphous Carbon", Veerasamy et al., Aug. 1993, pp. 319-326.-
  • "Fluorinated Diamond Like Carbon Films by Plasma Immersion Ion Processing Technique, Hakovirta et al., Mat. Res. Soc. Symp. Proc. vol. 593, pp. 285-290 (2000).".