Abstract
A method of fabricating a ferroelectric capacitor is disclosed. The method comprises the patterning of a top electrode layer and a dielectric layer to form a capacitor stack structure having sidewalls associated therewith. Prior to patterning the bottom electrode layer, a protective film is formed on the sidewalls of the capacitor stack structure in order to protect the dielectric material from conductive contaminants associated with a subsequent patterning of the bottom electrode layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 46.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming an FeRAM capacitor, comprising: forming a bottom diffusion barrier layer over a substrate; forming a bottom electrode layer over the bottom diffusion barrier layer; forming a ferroelectric dielectric layer over the bottom electrode layer; forming a top electrode layer over the ferroelectric dielectric layer; patterning the top electrode layer and the ferroelectric dielectric layer to form a capacitor stack structure having a top portion and sidewalls associated therewith, the capacitor stack structure overlying a first portion of the bottom electrode layer and leaving a sec
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 46 total)
References Cited — Backward Prior Art (9)
Non-Patent Literature (2)
- "A Survey of Circuit Innovations in Ferroelectric Random Access Memories", Ali Sheikholeslami and P. Glenn Gulak, Proceedings of the IEEE, vol. 88, No. 5, May, 2000, pp. 667-689.
- "FeRAM Tutorial", Ali Sheikholeslami and P. Glenn Gulak, A Survey of circuit innovations in Ferroelectric random-access memoies, Proceedings of the IEEE, vol. 88, No. 3, May, 2000, 3 pages, taken from the Internet at http://www.eecg.toronto.edu/-ali/ferro/tutorial.html.