Patents
US 6,627,313 B2#15362082 Most CitedExpiredUnited States (USPTO)Utility

Spindle-shaped magnetic metal particles containing iron as main component and processes for producing the same

7Forward Citations (#15362082 Global)
0.3/yrCitation Velocity (#25542661 Global)
1.72Citation PageRank (#18548957 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Spindle-shaped magnetic metal particles containing iron as a main component of the present invention, have an average major axis diameter (L) of 0.05 to 0.15 μm; a coercive force of 111.4 to 143.2 kA/m; a Co content of from 0.5 to less than 5 atm % based on whole Fe; a crystallite size of from 150 to less than 170 Å; a ratio of Al to Co from 1.0:1 to less than 2.0:1; a specific surface area (S) represented by the formula: S ≦−160× L +65; an oxidation stability (Δσs) of saturation magnetization of not more than 5.0%; and an ignition temperature of not less than 140° C. The spindle-shaped magnetic metal particles containing iron as a main component, exhibit an adequate coercive force, and are excellent in dispersibility, oxidation stability and coercive force distribution despite fine particles, especially notwithstanding the particles have an average major axis diameter as small as 0.05 to 0.15 μm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 7.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Spindle-shaped magnetic metal particles containing iron as a main component, having an average major axis diameter (L) of 0.05 to 0.15 μm; an aspect ratio of 4:1 to 7.2:1; a coercive force of 111.4 to 142.2 kA/m; a Co content of from 0.5 to less than 5 atm % based on whole Fe; a crystallite size of from 150 to less than 170 Å; a ratio of Al to Co from 1.1:1 to less than 2.0:1; a specific surface area (S) represented by the formula: S ≦−160 ×L +65; an oxidation stability (Δσs) of saturation magnetization of not more than 5.0%; and an ignition temperature of not less than 140° C.

  2. Claim 2Depends on #1

    Spindle-shaped magnetic metal particles containing iron as a main component according to claim 1 , which have an Al content of from 5 to 10 atm % based on whole Fe and a rare earth element conte

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗