Plasma etching method
Abstract
The temperature of the specimen holder 6 in the vacuum container 1 is lowered with the thermal control unit 11 to adjust the temperature of the specimen 7 composed of a silicon substrate to a low temperature of 0° C. or lower. Then, trenches are formed in the specimen 7 by plasma etching using an etching gas comprising SF6 as the main constituent and optionally O2 as an additive. Thus, the etching rate and the yield can be increased in the trench formation in the silicon semiconductor substrate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A plasma etching method comprising forming trenches in a silicon semiconductor substrate by using a mask made of silicon oxide or silicon nitride or a composite film thereof, wherein the temperature of the silicon semiconductor substrate is maintained in a range of 0° C. to −50° C. and the trenches are formed by using a plasma etching gas comprising sulfur hexafluoride as the main constituent, oxygen and hydrogen bromide.
- Claim 2Depends on #1
The plasma etching method according to claim 1 , wherein the substrate is previously cooled before the beginning of etching.
- Claim 3Independent Claim
A plasma etching method comprising forming trenches in a silicon semiconductor substrate by using a mask made of silicon oxide or silicon nitride or a composite film thereof, wherein the temperature of the silicon semiconductor substrate is maintained at 0° C. or
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (13 of 13 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (1)
- "Rie Lag In Diffractive Optical Element Etching"; Microelectronic Engineering; (2000); 54(3-4); pp. 315-322; Ting et al.