Oxide powder and method for preparing the same, and product using the same
Abstract
Firstly, a powder matrix is kept in a fluent state, said powder matrix consisting of a first oxide having an absorbed water amount of 0.1 to 50%, an averaged particle diameter of 0.005 to 0.5 mum and a surface hydroxyl group number of 0.1 to 25 mumol/m2. Then, one or both of a halide and an alkoxide including metal or semi-metal identical with or different from the metal or semi-metal constituting said first oxide is allowed to contact with said powder matrix kept in the fluent state, by means of an inert carrier gas, and then they are heated at a temperature of from 25 to 800° C., to thereby coat said powder matrix by a coating layer consisting of a second oxide. Further, a reaction by-product consisting of one or both of a hydrogen halide or an alcohol generated by said contacting is heated at a temperature of from 200 to 1000° C. within the inert carrier gas to thereby eliminate the reaction by-product.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 14.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A manufacturing method of an oxide powder comprising the steps of: keeping a powder matrix in a fluent state, said powder matrix consisting of a first oxide composed of one or both of a metal oxide and a semi-metal oxide, or a composite or mixed oxide from those oxides, and having an absorbed water amount of 0.1 to 50%, an averaged particle diameter of 0.005 to 0.5 μm and a surface hydroxyl group number of 0.1 to 25 μmol/m 2 ; contacting, one or both of a halide and an alkoxide including metal or semi-metal identical with or different from the metal or semi-metal constituting said first oxide,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗