Patents
US 6,613,638 B2#6110402 Most CitedExpiredUnited States (USPTO)Utility

Soi annealing method for reducing HF defects, with lamp, without crystal original particle (COP)

15Forward Citations (#6110402 Global)
0.7/yrCitation Velocity (#12168728 Global)
3.87Citation PageRank (#5016221 Global)
15Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The HF defect density in an SOI is reduced. After annealing step (S2) of annealing an SOI at a temperature between the melting point (e.g., 993° C.) of a semiconductor metal compound (e.g., nickel silicide) formed from a metal and the semiconductor material of the crystal semiconductor of the SOI (inclusive) and the melting point of the semiconductor material (inclusive), the temperature is reduced such that the cooling rate within the temperature range from the melting point of the semiconductor metal compound and the production temperature (e.g., 775° C.) of the semiconductor metal compound becomes 0.12° C./sec or more.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 15.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An SOI annealing method comprising the steps of: annealing an SOI at a temperature from 993° C. to a melting point of silicon, wherein a nickel concentration on a surface of the SOI is not less than 1×10 9 atoms/cm 2 ; and reducing a temperature of the SOI after the annealing step, wherein a cooling rate within a temperature range from 993° C. to 775° C. is not less than 0.12° C./sec.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the cooling rate is not less than 3° C./sec.

  3. Claim 3Depends on #1

    The method according to claim 1 , wherein the cooling rate is not less than 6° C./sec.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 15 total)

PatentTitleYearCitations
US 8,822,242 B2Methods for monitoring the amount of metal contamination in a process20140
DE 112010004811 B4Verfahren zur Herstellung eines Silizium-Epitaxiewafers20210
US 8,143,078 B2Methods for monitoring the amount of contamination imparted into semiconductor wafers during wafer processing20124
CN 102,687,260 AMethod for monitoring the amount of contamination imparted into semiconductor wafers during wafer processing—11
US 2011151592 A1Methods for monitoring the amount of contamination imparted into semiconductor wafers during wafer processing—12
US 2004207016 A1CMOS-compatible integration of silicon-based optical devices with electronic devices—46
US 2011212550 A1Methods for detecting metal precipitates in a semiconductor wafer—2
US 2002086463 A1Means for forming SOI—26
US 2002160208 A1SOI substrate, annealing method therefor, semiconductor device having the SOI substrate, and method of manufacturing the same—4
US 6,968,110 B2CMOS-compatible integration of silicon-based optical devices with electronic devices200578
US 7,101,772 B2Means for forming SOI20066
US 2003057489 A1Method for manufacturing semiconductor substrate, semiconductor substrate, electrooptic device and electronic apparatus—24
US 2011212547 A1Methods for monitoring the amount of metal contamination imparted into wafers during a semiconductor process—1
US 8,058,149 B2Method for fabricating a semiconductor substrate20110
US 2005236619 A1CMOS-compatible integration of silicon-based optical devices with electronic devices—29

Non-Patent Literature (1)

  • D.K. Sadana et al., "Nano-Defects in Commercial Bonded SOI and SIMOX," Proceedings 1994 IEEE International SOI Conference, pp. 111-112 (1994).